| 1843 - 750 lapas
...deposited ; and, so perfect is the sheet of copper thus formed, that, being stript off, it has the counterpart of every scratch of the plate on which it is deposited.' This paper seems to have attracted very little attention ; and, what seems still more singular, the... | |
| 1841 - 542 lapas
...ignited for four hours. The zinc plate is always partially covered with a coating of copper, which, however, is NOT DETRIMENTAL to the power of the battery...hydrogen, being set at liberty. This may be readily shewn by soldering at one end a piece of copper and a piece of zinc, coiling the two to form a small... | |
| William Savage - 1841 - 836 lapas
...4>84°,) where he says, " The zinc plate is always partially covered with a coating of copper, which, however, is not detrimental to the power of the battery...every scratch of the plate on which it is deposited." The discovery of the application is claimed by two persons, M. Jacobi, a Russian, and Mr. Thomas Spencer... | |
| Alfred Smee - 1841 - 306 lapas
...deposited ; and so perfect is the sheet of copper thus formed, that being stripped off, it has the counterpart of every scratch of the plate on which it is deposited." This paper appears to have attracted very little attention; and what appears still more singular, the... | |
| 1843 - 314 lapas
...deposited ; and so perfect is the sheet of copper thus formed, that, being stripped off, it has the counterpart of every scratch of the plate on which it is deposited." This paper seems, however, to have attracted but little attention, and the author does not appear to... | |
| Alfred Smee - 1843 - 378 lapas
...deposited; and so perfect is the sheet of copper thus formed, that, being stripped off, it has the counterpart of every scratch of the plate on which it is deposited." This paper seems to have attracted very little attention ; and, what seems still more singular, the... | |
| Perry Fairfax Nursey - 1844 - 474 lapas
...coating of copper, which, however, is not detrimental to the power of the battery ; the copper-plate is also covered with a coating of metallic copper,...every scratch, of the plate on which it is deposited." Mr. De la Rue makes this remark incidentally, and I only offer it here as a proof how near others have... | |
| 1844 - 544 lapas
...coating of copper, which, however, is not detrimental to the power of the battery ; the copper-plate is also covered with a coating of metallic copper,...every scratch, of the plate on which it is deposited." Mr. De la Rue makes this remark incidentally, and I only offer it here as a proof how near others have... | |
| Henry Minchin Noad - 1844 - 512 lapas
...a coating of metallic copper, which is continually being deposited ;" and he proceeds to remark, " so perfect is the sheet of copper thus formed, that...every scratch of the plate on which it is deposited." On reading this passage at the present time, when the art of Electro-metallurgy is so extensively practised,... | |
| 1844 - 490 lapas
...with a coating of metallic copper, which is continually being deposited ; and io perfect is the theet of copper thus formed, that, on being stripped off,...every scratch, of the plate on which it is deposited." Mr. De la Rue makes this remark incidentally, and I only offer it here as a proof how near others have... | |
| |